WD PUR Hot Melt Adhesive for Woodworking Flat Lamination | 100% Solids, Moisture-Curing Polyurethane Adhesive
Product Overview
WD is a moisture-curing reactive polyurethane hot melt adhesive with 100% solids, primarily intended for wood flat lamination, including WPC board flat lamination. It provides initial strength after cooling to support subsequent processing, with heat and water resistance after full cure.
Problem | How Can Processing Speed and Bond Performance Be Assessed Together?
Wood flat lamination requires more than checking whether the surfaces hold together after pressing. Subsequent processing and performance after curing also matter. WD provides initial strength after cooling, but this initial setting does not directly establish final heat and water resistance. Initial positioning and cured bond performance should be assessed separately.
Cause | Initial Strength and Cured Performance Develop at Different Stages
WD uses a moisture-reactive polyurethane hot melt system. Cooling after application helps establish initial strength, while subsequent moisture curing contributes to final property development. Inspection immediately after pressing therefore cannot replace testing after curing. A recommended waiting period before testing should not automatically be interpreted as a full-cure time.
Solution | Record Temperature, Viscosity and the Interval Before Pressing
During trials, record the substrate combination, actual application temperature and interval before pressing. The documented melt viscosity is 15,000±3,000 mPa·s at a measurement temperature of 120°C. The stated open time is 4±2 minutes, but the test conditions are unspecified. Confirm the actual processing window through production-line lamination trials.
Technical Specifications
|
Parameter |
Value or Description |
Conditions and Notes |
|---|---|---|
|
Product Model |
WD |
Model listed in the document |
|
Chemical Composition |
Reactive polyurethane hot melt adhesive |
PUR hot melt system |
|
Curing Mechanism |
Moisture-curing |
Equipment sealing and air exposure require attention |
|
Solids Content |
100% |
Stated value |
|
Color |
Water-white |
Visual inspection |
|
Density |
1.1±0.05 g/cm³ |
Test standard listed: GB/T 13477-2002 |
|
Melt Viscosity |
15,000±3,000 mPa·s |
At 120°C; ISO 3219 |
|
Open Time |
4±2 min |
Test conditions not specified |
|
Softening Temperature |
85±5°C |
Does not establish maximum service temperature after curing |
|
Application Temperature |
120–150°C in the specification table; 110–150°C in the operating instructions |
Inconsistent ranges; clarification required |
|
Peel Force on PVC |
≥40 N/25 mm |
Complete specimen construction and test conditions not specified |
|
Packaging |
20 kg/drum or 170 kg/drum |
As stated in the document |
|
Storage Conditions |
Cool, dry conditions at 10–25°C |
As stated in the storage instructions |
|
Shelf Life |
6 months in original packaging |
As stated in the document |
Application | Wood and WPC Board Flat Lamination
The document identifies wood flat lamination and specifically lists WPC board flat lamination. The stated peel force on PVC of ≥40 N/25 mm can serve as a reference for relevant trials. However, without the complete laminated construction and test conditions, this value does not establish suitability for every PVC film and board combination.
How to Choose | Confirm the Materials Before Establishing Processing Conditions
First identify the board and facing materials, then check equipment sealing and application temperature. The document gives two temperature ranges: 110–150°C and 120–150°C. Clarification is required before use. It also warns that temperatures above 150°C may deform PVC film.
FAQ | Does a 24-Hour Waiting Period Establish Full Cure?
No. The document only recommends testing assembled panels after 24 hours; it does not specify a full-cure time. The softening temperature of 85±5°C also does not establish the heat-resistance limit after curing. Service-temperature assessments require appropriate test evidence.