logo

Rear Window Automotive Rtv Sealant High Temp Sealant

Place of Origin: China
Brand Name: YT
Certification: ISO9001, Work safety standardization certificate
Model Number: Automotive Adhesive
Minimum Order Quantity: 50 metric tons
Price: Custom Product Production
Delivery Time: Customized production depends on the situation.
Payment Terms: L/C, D/A, D/P, T/T, Western Union
Supply Ability: Custom Product Production
Inquiry Now
Get A Quote
Specifications
Highlight Features

Rear Window automotive rtv sealant

,

oem automotive rtv sealant 1.85MPa

,

1.85MPa high temp sealant automotive

Product Name:
Electric Microcar Rear Window Silicone Sealant
Grade:
4C / 5C / 6C
Density:
1.5–1.7 G/cm³
Hardness:
50–65 Shore A, Depending On Grade
Tensile Strength:
1.4–2.0 MPa, Depending On Grade
Skin-Over Time:
20–40 Min, Depending On Grade
Cure Rate:
1.2–3 Mm/24h, Depending On Grade
Application:
Bonding And Sealing Glass-to-Metal Frame Joints In Low-Speed EVs
Product Description

Electric Microcar Rear Window Silicone Sealant For Glass-To-Frame Bonding And Sealing

 

Problem | Why Should a Rear Window Not Be Sealed in the Same Way as a Simple Straight Glass Joint?

The rear window of an electric microcar is typically installed within a tailgate frame that contains changes in contour and direction. Unlike a simple straight joint, the sealant path needs to continue around the entire glass perimeter, including corners, curved edges and frame transitions.

The main issue is not simply whether sealant is present. The bead needs to remain continuous around the perimeter and correspond to the actual assembly gap.

Along a straight edge, nozzle angle and travel speed can remain relatively stable. At a corner, however, the dispensing direction changes. If material flow, nozzle distance and travel speed are not coordinated, the bead can become thinner, accumulate locally or lose continuity.

The complete perimeter should therefore be evaluated rather than checking only one visible section.

 

Cause | Why Do Rear Window Corners and Bead Start/End Points Require Additional Inspection?

 

Corners change the dispensing direction, while a perimeter bead also requires its start and end points to connect correctly.

If this connection is incomplete, an otherwise uniform bead can still contain a local interruption.

Curing also requires separate consideration. 4C and 5C have specified skin-over times of 20–40 minutes, while 6C is 20–30 minutes. The specified cure rate is 1.5–3 mm/24h for 4C and 1.2–3 mm/24h for 5C and 6C.

Where a local assembly gap produces a deeper sealant section, the material can therefore continue curing internally after the exposed surface has formed a skin.

 

Solution | How Should 4C, 5C and 6C Be Selected for a Rear Window Assembly?

 

First identify the actual glass surface, tailgate-frame material and frame surface condition. Then measure joint width and depth around the perimeter and inspect the corner geometry and bead connection point.

The product grades can then be compared using their documented properties.

4C provides 50–60 Shore A hardness and 1.85 MPa tensile strength. 5C provides 65 Shore A hardness and 1.4–1.6 MPa tensile strength. 6C provides 60 Shore A hardness and 1.9–2.0 MPa tensile strength.

Neither hardness nor tensile strength alone establishes which grade is suitable for every rear window design.

A practical process is:

Glass and Frame Identification → Perimeter Joint Measurement → Corner Inspection → 4C/5C/6C Property Comparison → Continuous Dispensing → Cure Management → Actual Tailgate Assembly Verification

 

How It Works | How Does Silicone Sealant Create a Continuous Seal Around an LSEV Rear Window?

 

Silicone sealant is continuously dispensed along the interface between the rear glass and tailgate frame, filling the actual assembly gap to create a complete perimeter bead.

Straight sections require consistent bead dimensions. At corners and curved edges, nozzle direction changes while material flow should remain continuous.

The start/end connection of the perimeter bead should also be inspected separately to avoid an obvious interruption.

For deeper sections, downstream processing should take the specified cure rate into account: 1.5–3 mm/24h for 4C and 1.2–3 mm/24h for 5C and 6C. Surface skin formation alone should not be treated as evidence of complete internal curing.

 

FAQ | What Are the Common Sealant Selection Questions for an LSEV Rear Window?

 

Does a tack-free surface mean that the entire rear window bead is fully cured?
No. Skin-over time and internal curing describe different stages. Joint depth and the specified cure rate should also be considered.

Does the shorter 20–30 minute skin-over time make 6C automatically more suitable than 4C or 5C?
No. Skin-over time is only one parameter. Hardness, tensile strength, joint geometry and the actual substrates should also be considered.

Can the sealant be claimed to work with every rear window and metal frame?
The supplied information supports glass bonding and sealing applications, but it does not provide specific adhesion data for every glass surface and metal coating combination. Actual assembly verification is therefore recommended.

 

Technical Specifications

 

 

Property

4C

5C

6C

Appearance

Uniform Black Paste

Uniform Black Paste

Uniform Black Paste

Density at 25°C

1.5–1.7 g/cm³

1.5–1.7 g/cm³

1.5–1.7 g/cm³

Volatile Content at 150°C

3–4%

3–4%

3–4%

Hardness

50–60 Shore A

65 Shore A

60 Shore A

Tensile Strength

1.85 MPa

1.4–1.6 MPa

1.9–2.0 MPa

Skin-Over Time

20–40 min

20–40 min

20–30 min

Cure Rate

1.5–3 mm/24h

1.2–3 mm/24h

1.2–3 mm/24h