logo

LSEV Automotive Sealant Lower Edge Windshield Silicone Sealant For Bonding And Sealing

Place of Origin: China
Brand Name: YT
Certification: ISO9001, Work safety standardization certificate
Model Number: Automotive Adhesive
Minimum Order Quantity: 50 metric tons
Price: Custom Product Production
Delivery Time: Customized production depends on the situation.
Payment Terms: L/C, D/A, D/P, T/T, Western Union
Supply Ability: Custom Product Production
Inquiry Now
Get A Quote
Specifications
Highlight Features

LSEV Automotive Sealant

,

Bonding Automotive Sealant

,

Sealing Windshield Silicone Sealant

Product Name:
LSEV Windshield Lower Edge Silicone Sealant
Grade:
4C / 5C / 6C
Density:
1.5–1.7 G/cm³
Hardness:
50–65 Shore A, Depending On Grade
Tensile Strength:
1.4–2.0 MPa, Depending On Grade
Skin-Over Time:
20–40 Min, Depending On Grade
Cure Rate:
1.2–3 Mm/24h, Depending On Grade
Application:
Bonding And Sealing Glass-to-Metal Frame Joints In Low-Speed EVs
Product Description

LSEV Windshield Lower Edge Silicone Sealant For Glass-To-Frame Bonding And Sealing

 

Problem | Why Should the Lower Windshield Edge Not Be Treated as Just Another Simple Perimeter Glass Joint?

 

Although the windshield of a Low-Speed Electric Vehicle (LSEV) is a glass bonding and sealing application, its lower edge can present a different dispensing condition from a simple straight glass joint.

The lower glass edge may form a relatively long continuous interface with the body frame before transitioning into the two lower corners. As a result, bead direction, joint width and available dispensing space can change along the application path.

If the same material flow is maintained without adapting nozzle movement to the actual joint, a stable bead along the straight section may become thinner or accumulate excessively near the corners.

The objective is therefore to confirm a continuous bonding and filling path across the lower glass edge, both corners and adjacent frame interfaces.

 

Cause | Why Can Different Areas Along the Windshield Lower Edge Develop Different Bead Cross-Sections?

 

Along a straight section, nozzle angle and travel speed are relatively easy to maintain. When the application reaches a lower windshield corner, the dispensing direction changes and the distance between the nozzle and joint can also vary.

If material flow is not coordinated with these movements, the bead cross-section can change.

Joint depth also affects curing management. 4C and 5C have specified skin-over times of 20–40 minutes, while 6C is 20–30 minutes. The specified cure rate is 1.5–3 mm/24h for 4C and 1.2–3 mm/24h for 5C and 6C.

A surface skin therefore does not demonstrate that a deeper section has reached the same curing condition.

 

Solution | How Should 4C, 5C and 6C Be Compared for an LSEV Windshield Lower-Edge Application?

 

Begin by identifying the actual glass surface, body-frame material and surface condition. Measure joint width and depth along the windshield lower edge, with particular attention to both lower corners and areas where the assembly gap changes.

The documented product properties can then be compared.

4C provides 50–60 Shore A hardness and 1.85 MPa tensile strength. 5C provides 65 Shore A hardness and 1.4–1.6 MPa tensile strength, while 6C provides 60 Shore A hardness and 1.9–2.0 MPa tensile strength.

The higher hardness value of 5C does not by itself establish overall superiority, just as the higher specified tensile-strength range of 6C does not automatically make it suitable for every windshield structure.

A practical selection process is:

Glass Surface → Frame Surface → Lower-Edge Joint Dimensions → Corner Geometry → 4C/5C/6C Property Comparison → Sample Application → Cure Management → Actual Windshield Assembly Verification

 

How to Choose | Which Parameters Should Be Evaluated Together for an LSEV Windshield Lower-Edge Joint?

 

Joint geometry should be evaluated before selecting a grade from individual material properties.

For hardness, compare 50–60 Shore A for 4C, 65 Shore A for 5C and 60 Shore A for 6C. Their tensile strengths are 1.85 MPa, 1.4–1.6 MPa and 1.9–2.0 MPa, respectively.

Where production timing is sensitive to surface skin formation, the 20–40 minute skin-over time of 4C/5C can be compared with the 20–30 minute value of 6C.

For deeper lower-edge joints, downstream processing should also consider the specified 1.5–3 mm/24h or 1.2–3 mm/24h cure rate.

Hardness, tensile strength, skin-over time and cure rate should therefore be considered together with actual joint dimensions.

 

Application Scenarios | Which LSEV Windshield Lower-Edge Joints Are Suitable for This Application?

 

This application is intended for the lower windshield connection areas of Low-Speed Electric Vehicles (LSEVs) and electric microcars, including long glass-to-frame interfaces, lower left and right corners, and sections where the assembly gap changes locally.

The supplied product information supports glass bonding and sealing in low-speed electric vehicle applications, providing a basis for this dedicated application page.

However, the available information does not contain specific adhesion data for every glass surface treatment, metal substrate or body-frame coating combination. Claims of universal compatibility should therefore be avoided, and the actual glass and frame assembly should be verified before volume production.

 

Technical Specifications

 

 

Property

4C

5C

6C

Appearance

Uniform Black Paste

Uniform Black Paste

Uniform Black Paste

Density at 25°C

1.5–1.7 g/cm³

1.5–1.7 g/cm³

1.5–1.7 g/cm³

Volatile Content at 150°C

3–4%

3–4%

3–4%

Hardness

50–60 Shore A

65 Shore A

60 Shore A

Tensile Strength

1.85 MPa

1.4–1.6 MPa

1.9–2.0 MPa

Skin-Over Time

20–40 min

20–40 min

20–30 min

Cure Rate

1.5–3 mm/24h

1.2–3 mm/24h

1.2–3 mm/24h

Related Products