Quick Link
Quick Contact
Address
No. 1707, Industrial Road, Tangshan Town, Huantai County, Zibo City, Shandong Province
Tel
86-533-17860959591
Our Newsletter
Subscribe to our newsletter for discounts and more.
LSEV Quarter Window Silicone Sealant For Fixed Glass-To-Body Frame Bonding And Sealing
Problem | Why Does a Non-Moving Quarter Window Still Require Careful Control of the Perimeter Joint?
Unlike movable door glass, some low-speed electric vehicles use fixed rear side windows. Although the glass remains stationary after installation, its perimeter joint should not be treated as a simple straight sealing line.
A fixed window can contain straight edges, inclined sections, curved profiles and multiple corners. The dispensing path therefore changes continuously around the glass perimeter.
If inspection focuses only on whether a bead forms a complete visible circle around the glass, variations in the actual bead cross-section can be overlooked.
The main objective is continuous perimeter bead formation and consistent filling of the actual glass-to-body-frame interface.
Cause | Why Are Quarter-Window Corners and Inclined Edges More Likely to Develop Variations in Bead Cross-Section?
Along a long straight edge, nozzle speed, angle and material delivery can be maintained more consistently. When the bead enters an inclined edge, curved profile or corner, the dispensing direction needs to change.
If nozzle movement slows while material flow remains unchanged, local accumulation can occur. If movement becomes too fast during the directional transition, a thinner bead section may result.
Joint depth can also vary around the window perimeter. 4C and 5C specify 20–40 minutes skin-over time, while 6C specifies 20–30 minutes. Cure rates are 1.5–3 mm/24h for 4C and 1.2–3 mm/24h for 5C and 6C.
A surface skin therefore does not demonstrate that deeper areas have reached the same curing condition.
Solution | How Should 4C, 5C and 6C Be Selected According to Quarter-Window Joint Geometry?
First identify the actual fixed-glass surface, body-frame material and surface condition. Joint width and depth should then be checked along straight edges, inclined sections and corners.
The three grades can subsequently be compared.
4C provides 50–60 Shore A hardness and 1.85 MPa tensile strength. 5C provides 65 Shore A hardness and 1.4–1.6 MPa tensile strength, while 6C provides 60 Shore A hardness and 1.9–2.0 MPa tensile strength.
Because these grades provide different combinations of hardness, tensile strength, skin-over time and cure rate, the grade numbers should not be treated as a simple performance ranking.
A practical selection sequence is:
Fixed Glass Surface → Body-Frame Surface → Perimeter Joint Width/Depth → Corner and Inclined-Edge Geometry → 4C/5C/6C Properties → Sample Application → Cure Management → Actual Quarter-Window Assembly Verification
How It Works | How Does Silicone Sealant Form a Continuous Bonding and Sealing Path Around a Fixed Quarter Window?
Black silicone sealant is continuously applied along the required connection between the fixed glass and body frame, filling the actual assembly joint to create a perimeter sealing path.
Along long straight sections, nozzle travel speed and material delivery should be coordinated. At inclined edges, curved profiles and corners, nozzle direction should follow the glass geometry.
The start/end connection of the perimeter bead should also be checked. A thicker bead in one area cannot compensate for a discontinuity elsewhere.
Where joint depth varies, downstream operations should consider the specified cure rate rather than using skin-over time as an indication of complete curing.
FAQ | What Are the Common Sealant Selection Questions for an LSEV Quarter Window?
Does a fixed window only require consideration of sealant hardness because the glass does not move?
No. Joint dimensions, tensile strength, skin-over time and cure rate should also be evaluated.
Does the 20–30 minute skin-over time of 6C mean that the entire bead necessarily cures faster?
No. Skin-over time and cure rate are different parameters. 6C specifies a cure rate of 1.2–3 mm/24h, and actual internal curing also depends on bead depth.
Can the product be described as universally suitable for all fixed glass and body-frame combinations?
The available information supports glass bonding and sealing in low-speed electric vehicle applications, but does not provide dedicated adhesion data for every glass treatment, metal or coating combination. Actual component verification is therefore appropriate.
Technical Specifications
|
Property |
4C |
5C |
6C |
|---|---|---|---|
|
Appearance |
Uniform Black Paste |
Uniform Black Paste |
Uniform Black Paste |
|
Density at 25°C |
1.5–1.7 g/cm³ |
1.5–1.7 g/cm³ |
1.5–1.7 g/cm³ |
|
Volatile Content at 150°C |
3–4% |
3–4% |
3–4% |
|
Hardness |
50–60 Shore A |
65 Shore A |
60 Shore A |
|
Tensile Strength |
1.85 MPa |
1.4–1.6 MPa |
1.9–2.0 MPa |
|
Skin-Over Time |
20–40 min |
20–40 min |
20–30 min |
|
Cure Rate |
1.5–3 mm/24h |
1.2–3 mm/24h |
1.2–3 mm/24h |