LSEV Hood Panel Silicone Sealant For Inner-To-Outer Panel Hem And Seam Sealing
Problem | Why Does a Hemmed Hood Still Require Continuous Sealing Control Around the Inner-to-Outer Panel Joint?
A low-speed electric vehicle hood can be assembled from an outer panel and internal sheet-metal components. Although the perimeter may form a relatively long hemmed connection, the actual joint is not a completely uniform straight line.
The left and right sides may contain long regular sections, while the front, rear and corner areas introduce changes in direction. Local hem width and overlap depth may also vary.
If the same nozzle angle and travel speed are maintained without adapting to these structural changes, filling conditions can vary between straight sections and corners.
The main control point is therefore continuous sealant application along the inner-to-outer panel connection and consistent filling where long edges transition into corners.
Cause | Why Are Hood Corners and Local Overlap Sections More Likely to Develop Variations in Sealant Thickness?
Along a long straight hem, nozzle movement and material delivery can usually be controlled relatively consistently.
At a corner, however, the nozzle must change direction. If travel speed decreases without a corresponding change in material delivery, a thicker local bead can form. If the nozzle moves too quickly through the turn, the amount of sealant entering the joint can decrease.
Surface skin formation should also be distinguished from internal curing where joint depth varies.
4C and 5C specify 20–40 minutes skin-over time, while 6C specifies 20–30 minutes. Cure rates are 1.5–3 mm/24h for 4C and 1.2–3 mm/24h for 5C and 6C.
A similar surface appearance therefore does not necessarily mean that every joint section has reached the same internal curing condition.
Solution | How Should 4C, 5C and 6C Be Selected According to Hood Hem-Joint Geometry?
The actual hood construction should first be inspected, including the inner-to-outer panel connection, surface condition, perimeter hem width, local overlaps and corner geometry.
The documented properties can then be compared according to actual joint dimensions.
4C provides 50–60 Shore A hardness and 1.85 MPa tensile strength. 5C provides 65 Shore A hardness and 1.4–1.6 MPa tensile strength, while 6C provides 60 Shore A hardness and 1.9–2.0 MPa tensile strength.
For a long perimeter sealing path, skin-over time should also be considered in relation to the application process. For deeper local joints, cure rate becomes an additional process consideration.
A practical sequence is:
Hood Panels → Surface Condition → Hem/Overlap Geometry → Joint Width and Depth → 4C/5C/6C Properties → Sample Application → Cure Management → Actual Hood Assembly Verification
How It Works | How Does Silicone Sealant Form a Continuous Sealing Path Along the Hood Inner-to-Outer Panel Joint?
Black silicone sealant is continuously dispensed along the hood inner-to-outer panel connection that requires filling and sealing.
Along long straight hem sections, material delivery and nozzle travel should remain coordinated. At front, rear and side corners, nozzle direction should follow the actual panel geometry so that the sealant continues into the joint.
Where application stops and restarts, the connection between the two bead sections should also be checked rather than relying on excessive local material to compensate for an interrupted path.
For joints with different depths, downstream operations should consider the specified mm/24h cure rate rather than treating skin-over time as complete cure time.
How to Choose | Which Parameters Should Be Compared Together When Selecting a Sealant for Hood Panel Seams?
The first factor is joint geometry. Long straight edges and front/rear corners may have different widths and depths.
The second is hardness and tensile strength. The 65 Shore A hardness of 5C and the 1.9–2.0 MPa tensile strength of 6C represent different performance dimensions and should not be treated as interchangeable indicators.
The third factor is processing and curing behavior. 4C/5C and 6C have different skin-over times, while 4C and 5C/6C also have different specified cure-rate ranges.
The available product information does not provide dedicated adhesion data for every body metal, coating and surface-treatment system. Verification using the actual hood components is therefore appropriate before establishing the production process.
Technical Specifications
|
Property |
4C |
5C |
6C |
|---|---|---|---|
|
Appearance |
Uniform Black Paste |
Uniform Black Paste |
Uniform Black Paste |
|
Density at 25°C |
1.5–1.7 g/cm³ |
1.5–1.7 g/cm³ |
1.5–1.7 g/cm³ |
|
Volatile Content at 150°C |
3–4% |
3–4% |
3–4% |
|
Hardness |
50–60 Shore A |
65 Shore A |
60 Shore A |
|
Tensile Strength |
1.85 MPa |
1.4–1.6 MPa |
1.9–2.0 MPa |
|
Skin-Over Time |
20–40 min |
20–40 min |
20–30 min |
|
Cure Rate |
1.5–3 mm/24h |
1.2–3 mm/24h |
1.2–3 mm/24h |