Water White Industrial Moisture Curing Hot Glue Stick Hot Melt Adhesives For Bonding

Place of Origin: China
Brand Name: YT
Certification: ISO9001,
Model Number: Hot Helt Adhesives
Inquiry Now
Get A Quote
Specifications
Highlight Features

water white hot helt adhesives

,

hot helt adhesives moisture curing

,

moisture curing industrial hot glue

Product Name:
PUR Hot Melt Adhesive For Woodworking Flat Lamination
Chemistry And Cure:
Reactive Polyurethane Hot Melt Adhesive; Moisture-curing
Melt Viscosity:
15,000±3,000 MPa·s At 120°C; ISO 3219
Open Time:
4±2 Min
Application Temperature:
120–150°C In The Specification Table; 110–150°C In The Operating Instructions; Clarification Required
Peel Force On PVC:
≥40 N/25 Mm
Solids Content:
100%
Application:
Wood Flat Lamination And WPC Board Flat Lamination
Product Description

PUR Hot Melt Adhesive for Wood and WPC Board Flat Lamination

 

Product Overview

 

WD is a moisture-curing reactive polyurethane hot melt adhesive with 100% solids, primarily intended for woodworking flat lamination, including WPC board flat lamination. It provides initial strength after cooling to support subsequent operations, with heat and water resistance after full cure.

 

Problem | Why Is Heating Temperature Alone Insufficient for Adhesive Selection?

 

Woodworking flat lamination requires attention to adhesive application conditions, the temperature limitations of facing materials and subsequent processing requirements. Although WD is applied as a hot melt adhesive, heating capability alone does not establish suitability. Processes involving PVC film must also account for the high-temperature deformation risk identified in the document.

 

Cause | Application, Measurement and Service Temperatures Have Different Meanings

 

The stated 120°C is the measurement temperature for melt viscosity, while 85±5°C is the softening temperature. Neither directly establishes the service-temperature range after curing. The document does not specify a continuous heat-resistance temperature, so its description of heat resistance after full cure should not be converted into a temperature-specific service commitment.

 

Solution | Clarify the Temperature Range Before Establishing the Processing Sequence

 

The operating instructions state 110–150°C, while the specification table states 120–150°C. The different lower limits require clarification before use. During trials, record the actual application temperature, substrate combination and interval before pressing. Evaluate the processing sequence with reference to the stated open time of 4±2 minutes, rather than directly applying a value with unspecified test conditions to the production line.

 

Technical Specifications

 

Parameter

Value or Description

Chemical Composition

Reactive polyurethane hot melt adhesive

Curing Mechanism

Moisture-curing

Solids Content

100%

Color

Water-white

Density

1.1±0.05 g/cm³

Melt Viscosity

15,000±3,000 mPa·s

Open Time

4±2 min

Softening Temperature

85±5°C

Application Temperature

120–150°C in the specification table; 110–150°C in the operating instructions

Peel Force on PVC

≥40 N/25 mm

Packaging

20 kg/drum or 170 kg/drum

Storage Conditions

Cool, dry conditions at 10–25°C

Shelf Life

6 months in original packaging

 

Application | Keep the Scope Specific to Woodworking Flat Lamination

 

The document identifies wood flat lamination and specifically lists WPC board flat lamination. The PVC-related peel-force value can serve as a reference for trials. However, the complete laminated construction is not specified, so it does not establish suitability for every PVC film and board combination or for specific furniture or building components.

 

How It Works | Initial Setting Must Be Distinguished from Full Cure

 

WD provides initial strength after cooling to support subsequent processing. Heat and water resistance are described for the fully cured adhesive. The document recommends testing assembled panels after 24 hours, but this period does not establish a full-cure time.

 

How to Choose | Validate the Actual Material Combination

 

First identify the board and facing materials, then check the application temperature and equipment sealing. The stated peel force on PVC of ≥40 N/25 mm can serve as a reference. Final suitability should be assessed using the actual laminated construction and test results after curing.